Hi Guy's n Girl's

Just a quick question about solder, which solder do you guys use?

Currently i've got some weller radiolot solder that im not overly impressed with get mixed results and its seems very corrosive flux in the solder attacks the iron tip.
So i'm looking for an alternative really.

I'm no eletrical engineer, but im no numpty either (apart from the wife opinion.....). perhaps its me! not being able to get used to this leadfree day's.

But anyway would greatly appreciate any imput on this?

Thanks in advance,
Shiny.
__________________
http://www.ebaumsworld.com/signs/sign1.jpg
Reply With Quote
  #2  
Old 18-07-2015
200sx 200sx is offline
Member
 
Join Date: Apr 2012
Location: Nottingham
Posts: 266
Default

MG Chemicals 63/37 no clean
Reply With Quote
  #3  
Old 18-07-2015
Lee1972's Avatar
Lee1972 Lee1972 is offline
Senior Member
 
Join Date: Jan 2011
Location: Darwen, Lancashire
Posts: 792
Default

I found lead free solder a pain in the rear so bought some leaded off ebay no problems now with my soldering
Reply With Quote
  #4  
Old 18-07-2015
joker's Avatar
joker joker is offline
Member
 
Join Date: May 2011
Posts: 150
Default

I've found the hudy solder to be great it gives great results every time
__________________
Roche p12 2017
Roche p10
Roche rapide f1
Zen rxgt12
Kyosho zx6.6
Reply With Quote
  #5  
Old 18-07-2015
SlowOne SlowOne is offline
Mad Member
 
Join Date: Oct 2007
Posts: 1,549
Default

Lead-free solder is a pain so go for lead solder and a good flux.

http://www.amazon.co.uk/gp/product/B...=1&*entries*=0

http://www.ebay.co.uk/itm/17079-Elec...-/281419054093

Do not use any flux paste with acid in, however small the amount. Clean excess flux off the joint with motor cleaner or similar.

Always use the flux on new joints to first tin them and then make the joint. Once the joint is made use the flux every so often to clean the joint. Repeated soldering of motor wires will create oxides that can give a dry joint. Re-tin the wire and post from time to time to keep the joint clean.

The resin-cored solder that is available isn't good enough. The flux evaporates almost immediately it is melted, so all it really does is clean the tip, not the joint! HTH
Reply With Quote
  #6  
Old 18-07-2015
Wig Wig is offline
Member
 
Join Date: Oct 2014
Location: Worcestershire
Posts: 193
Default

I have always used Silver solder (5% silver) for soldering stainless steel brass and copper for slot car chassis, making nimh battery packs, speedos, wires etc. Doesnt require flux and produces a nice clean joint everytime. Flux is corrosive and it is good practice to clean off the excess with water after though this is not always possible.

You do need a powerful iron though.
Reply With Quote
  #7  
Old 18-07-2015
shinytopman's Avatar
shinytopman shinytopman is offline
Member
 
Join Date: Nov 2006
Location: Medway
Posts: 257
Default

Thanks for that guys much appreciated.

Me thinks its time to buy a few and diff types and start experimenting, practice makes perfect as they say.
__________________
http://www.ebaumsworld.com/signs/sign1.jpg
Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT. The time now is 08:04 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2024, vBulletin Solutions, Inc.
oOple.com